Skip to content

Diamond Grinding

Reviewed by licensed engineers

Checked against its sources by licensed professional engineers on the previous site, where reviewers weren’t recorded by name.

How articles are reviewed

Diamond grinding (Figure 1) refers to a process where gang-mounted diamond saw blades (Figures 2 and 3) are used to shave off a thin, 1.5 - 19 mm (0.06 - 0.75 inch) top layer of an existing PCC surface in order to restore smoothness and friction characteristics. Most often, it is used to restore roadway friction or remove roughness caused by faulting, studded tire wear, and slab warping and curling.

Diamond grinding can reduce the IRI of an older pavement to 1.0 - 2.0 m/km (63 - 126 inches/mile).

Diamond Grinding Machine.Diamond Saw Blades.Gang-Mounted Diamond Saw Blades.
Figures 1–3. Diamond Grinding Machine. Diamond Saw Blades. Gang-Mounted Diamond Saw Blades.

Purpose

Corrective maintenance. Restores pavement smoothness and frictional characteristics. Can also be used in new construction to attain initial specified smoothness, although properly constructed PCC pavements should not require any diamond grinding.

Materials

Gang-mounted diamond saw blades.

Other Info

Diamond grinding addresses serviceability problems but not their root cause. For example, diamond grinding can substantially reduce the roughness on a faulted rigid pavement, but it will not address the cause of faulting, nor will it prevent roughness in the future as a result of additional faulting.

Because the grinding head is cooled with water, a byproduct of diamond grinding is a slurry of ground PCC particles and water. Most of this slurry is picked up by vacuums within the grinding machine and either deposited along the highway shoulder (in some rural areas) or collected in trucks for disposal.

Teaching this? Figures and worked examples are free to use with credit. How to cite

Cite this page

APA

Pavement Interactive. (2018, September 21). Diamond grinding. HeadLight. Retrieved [the date you read it], from https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/maintenance/diamond-grinding/

ASCE

Pavement Interactive. (2018). “Diamond Grinding.” HeadLight, <https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/maintenance/diamond-grinding/> ([the date you read it]).

BibTeX

@misc{pavint-diamond-grinding,
  author = {{Pavement Interactive}},
  title = {Diamond Grinding},
  year = {2018},
  publisher = {HeadLight},
  howpublished = {\url{https://pavementinteractive.org/reference-desk/maintenance-and-rehabilitation/maintenance/diamond-grinding/}},
  note = {Accessed [date]}
}
This address will not change. The citation records the date you read it.
Report an error

Reports go to the editors, who check them against the cited sources. Corrections are noted at the top of the article.

Only if you want a reply. It is not published.