Slab Stabilization/Slab Jacking

« Back to Glossary Index

Slab stabilization involves the restoration of support to slabs by filling voids, thereby reducing deflections. Slab jacking involves raising slabs to their desired elevation by pressure inserting material beneath settled slabs.