International Roughness Index (IRI)

« Back to Glossary Index

A measurement of the roughness of a pavement, expressed as the ratio of the accumulated suspension motion to the distance traveled obtained from a mathematical model of a standard quarter car traversing a measured profile at a speed of 50 mi/hr. (80 km/h).