The goal of pavement design is to specify the characteristics required for quality performance for a given application. Two key components are mix design and structural design. These processes must also take into account external parameters including subgrade characteristics, traffic loading, and the environment.

Featured Article

Grader placing UTPB_2

Water is sometimes called the “universal solvent” because given enough time, it will dissolve just about anything. Even something that appears pretty permanent, like an asphalt pavement, can be eroded and damaged by water action. Roads are still exposed to the elements, however, and it would be virtually impossible to keep a pavement from coming … Read more »