Structural HMA Overlays for PCC Pavement

HMA structural overlays are used to increase rigid pavement structural capacity. Therefore, they are considered rehabilitation, although they typically have some maintenance-type benefits as well. Although the specific constants used may be different, flexible overlays of rigid pavement are designed in the same basic manner as flexible overlays of flexible pavement.