Description

A difference in elevation across a joint or crack usually associated with undoweled JPCP. Usually the approach slab is higher than the leave slab due to pumping, the most common faulting mechanism. Faulting is noticeable when the average faulting in the pavement section reaches about 2.5 mm (0.1 inch). When the average faulting reaches 4 mm (0.15 in), diamond grinding or other rehabilitation measures should be considered (Rao et al., 19991).

Faulting - looking in the opposite direction of traffic flow.Faulting close-up.Faulting
Figures 1–3. Faulting - looking in the opposite direction of traffic flow. Faulting close-up. Faulting

Figure 4. Pumping and faulting failure mechanism described.

Problem

Roughness

Possible Causes

Most commonly, faulting is a result of slab pumping. Faulting can also be caused by slab settlement, curling and warping.

Repair

Faulting heights of less than 3 mm (0.125 inch) need not be repaired. Faulting in an undoweled JPCP between 3 mm (0.125 inch) and 12.5 mm (0.5 inch) is a candidate for a dowel bar retrofit. Faulting in excess of 12.5 mm (0.5 inches) generally warrants total reconstruction.

Teaching this? Figures and worked examples are free to use with credit. How to cite

Cite this page

APA

Pavement Interactive. (2021, July 20). Faulting. HeadLight. Retrieved [the date you read it], from https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/faulting/

ASCE

Pavement Interactive. (2021). “Faulting.” HeadLight, <https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/faulting/> ([the date you read it]).

BibTeX

@misc{pavint-faulting,
  author = {{Pavement Interactive}},
  title = {Faulting},
  year = {2021},
  publisher = {HeadLight},
  howpublished = {\url{https://pavementinteractive.org/reference-desk/pavement-management/pavement-distresses/faulting/}},
  note = {Accessed [date]}
}
This address will not change. The citation records the date you read it.
Sources (1)
  1. Rao et al. (1999). Longevity of Diamond-Ground Concrete Pavements. Transportation Research Record 1684. Transportation Research Board, National Research Council, Washington, D.C. pp. 128-136. ↩
Report an error

Reports go to the editors, who check them against the cited sources. Corrections are noted at the top of the article.

Only if you want a reply. It is not published.