Pavement Management
Pavement_Management_250

General Guidance

Print this pageEmail this to someoneShare on FacebookTweet about this on TwitterShare on Google+Share on LinkedInShare on RedditDigg this

Figure 1: US 101 in Washington state.

Figure 2: A two-lane highway in Hawaii

 

This is an informational resource on hot mix asphalt (HMA). It contains a general overview of all HMA aspects. It is intended to assist those who work with HMA in any way including architects, engineers, contractors, students, and homeowners.

Suggested Reading

  • Asphalt Institute. (2001[1]). HMA Construction. Manual Series No. 22 (MS-22). Asphalt Institute. Lexington, KY.
  • ASTM D 6433 – Standard Practice for Roads and Parking Lots Pavement Condition Index Surveys. From American Society for Testing and Materials (ASTM). (2000[2]). Annual Book of ASTM Standards, Section four: Construction. vol. 4.03. American Society for Testing and Materials. West Conshohocken, PA.
  • Transportation Research Board (TRB). (2000[3]). Hot-Mix Asphalt Paving Handbook 2000. Transportation Research Board, National Research Council. Washington, D.C.

Publications Cited

  • Asphalt Paving Association of Iowa (APAI). (no date given). Asphalt Paving Design Guide. APAI. West Des Moines, IA. http://www.apai.net.
  • Roberts, F.L., Kandhal, P.S., Brown, E.R., Lee, D.Y., and Kennedy, T.W. (1996[4]). Hot Mix Asphalt Materials, Mixture Design, and Construction. National Asphalt Paving Association Education Foundation. Lanham, MD.



Footnotes    (↵ returns to text)
  1. Annual Book of ASTM Standards, Section four: Construction.  vol. 4.03.  American Society for Testing and Materials.  West Conshohocken, PA.
  2. Hot Mix Asphalt Materials, Mixture Design, and Construction.  National Asphalt Paving Association Education Foundation.  Lanham, MD.

 

 

 

close citation

Thanks for sharing General Guidance.