Pavement Management
Pavement_Management_250

FWD AREA Parameter

Print this pageEmail this to someoneShare on FacebookTweet about this on TwitterShare on Google+Share on LinkedInShare on RedditDigg this

FWD tests produce a series of numbers that describes the deflection basin shape.  Although these numbers are descriptive, it is often desired to use a single number as a index of the deflection basin shape.  One such number, the AREA Parameter represents the normalized area of a vertical slice taken through a deflection basin between the center of the test load and 914 mm (3 feet) away from the test load.  Dividing the slice area by the deflection measured at the center of the test “normalizes” the AREA Parameter.  Thus the AREA Parameter is the length of one side of a rectangle where the other side of the rectangle is D0.  Figure 1 illustrates this concept.

Figure 1: The FWD AREA Parameter

The basic AREA Parameter equation is:

 
where: AREA = the FWD AREA Parameter.  Expressed in units of length (usually inches or mm).
D0 = surface deflection at the test load center
D1 = surface deflection at 12 inches from the test load center
D2 = surface deflection at 24 inches from the test load center
D3 = surface deflection at 36 inches from the test load center

Maximum and Minimum AREA Values

The maximum AREA value is 36 inches (915 mm) and would occur when all four deflection measurements are equal, which is not likely to actually occur.  For all four deflection measurements to be nearly equal the pavement would have to be extremely stiff (like rigid pavement or thick, full-depth HMA).  The equation for the maximum AREA value is as follows:

The minimum Area value should be no less than 11.1 in. (280 mm) and would occur when all pavement layers have the same elastic modulus.  Or, put another way, the pavement structure does not contribute any additional stiffness to the underlying subgrade.  This is highly unlikely for actual pavement structures.  Low AREA values suggest that the pavement structure is not much different from the underlying subgrade material.  This is not always a bad thing if the subgrade is extremely stiff, but this does not occur very often).  When all elastic moduli are equal the ratio of D1, D2 and D3 to D0 are as follows, which gives the minimum AREA value as shown below:

Typical AREA Values

Table 1 shows some typical AREA values.

Table 1: Some Typical AREA Values
Pavement AREA Value
inches mm
Rigid pavement 24 – 33 610 – 840
Thick flexible pavement
>= 100 mm (4 inches)
21 – 30 530 – 760
Thin flexible pavement
< 100 mm (4 inches)
16 – 21 410 – 530
BST 15 – 17 380 – 430
Weak BST 12 – 15 300 – 380

FWD Area Program

WSDOT has developed a program for the determination of the AREA Value and subgrade resilient modulus using the Dynatest FWD.

NOTES:

  • This program must be installed on to your computer before you can use it. During the installation you will be prompted to specify a location to which it can be installed. Once installed, the program and its supporting files take about 450 kB of disk space.
  • The program is designed for Windows operating systems.

The FWD Area program can also be downloaded from the Washington State DOT Materials Lab at: http://www.wsdot.wa.gov/biz/mats.

 

 

 

close citation

Thanks for sharing FWD AREA Parameter.