Pavement Management
Pavement_Management_250

Durability Cracking

Print this pageEmail this to someoneShare on FacebookTweet about this on TwitterShare on Google+Share on LinkedInShare on RedditDigg this

Description

Series of closely spaced, crescent-shaped cracks near a joint, corner or crack. It is caused by freeze-thaw expansion of the large aggregate within the PCC slab. Durability cracking is a general PCC distress and is not unique to pavement PCC.

Figure 1: D cracking at a slab

Problem

Some roughness, leads to spalling and eventual slab disintegration

Possible Causes

Freeze-thaw susceptible aggregate.

Repair

“D” cracking is indicative of a general aggregate freeze-thaw problem. Although a full-depth patch or partial-depth patch can repair the affected area, it does not address the root problem and will not, of course, prevent “D” cracking elsewhere.

 

 

 

close citation

Thanks for sharing Durability Cracking.